26.04.2023 08:09:33
|
EDF: Clarification on the stress corrosion phenomenon detected on parts of the auxiliary circuits of the main primary circuit of several nuclear reactors
Clarification on the stress corrosion phenomenon detected on parts of the auxiliary circuits of the main primary circuit of several nuclear reactors
On 10 March 2023, EDF proposed to the ASN (Nuclear safety authority) an evolution in its stress corrosion control strategy. EDF is accelerating the inspection of the concerned welds of the RIS and RRA systems, in order to include the elements identified on the weld repaired at Penly 11.
On 25 April 2023, the ASN announced to consider the schedule proposed by EDF for controls on priority welds to be appropriate2.
To date, the estimate of nuclear output in France for 2023 remains in the range 300-330TWh.
This press release is certified. Check its authenticity on medias.edf.com
About EDF
As a major player in energy transition, the EDF Group is an integrated energy company active in all businesses: generation, transmission, distribution, energy trading, energy sales and energy services. EDF group is a world leader in low-carbon energy, having developed a diverse production mix based mainly on nuclear and renewable energy (including hydropower). It is also investing in new technologies to support energy transition. EDF’s raison d’être is to build a net zero energy future with electricity and innovative solutions and services, to help save the planet and drive well-being and economic development. The Group is involved in supplying energy and services to approximately 40.3 million customers (1), of whom 30.3 million in France (2). It generated consolidated sales of €143.5 billion in 2021. EDF is listed on the Paris Stock Exchange.
(1) Since 2018, customers are counted per delivery site. A customer can have two delivery points: one for electricity and another one for gas.
(2) Including ÉS (Électricité de Strasbourg) and SEI.
1 See information note of 17 March 2023: (https://www.edf.fr/groupe-edf/agir-en-entreprise-responsable/notes-dinformation)
2 See press release of the ASN of 25 April 2023
Attachment
![](https://ml-eu.globenewswire.com/media/YzMxNjMxNzktZDQwMy00Mjg2LWExYzUtNzJkY2JjMjA0Mjc4LTEwMTEwMzg=/tiny/EDF.png)
![](https://images.finanzen.at/images/unsortiert/wertpapierdepot-absichern-aktienchart-boerse-750493204-260.jpg)
Wenn Sie mehr über das Thema Aktien erfahren wollen, finden Sie in unserem Ratgeber viele interessante Artikel dazu!
Jetzt informieren!
Nachrichten zu EDF (Electricité de France)mehr Nachrichten
16.02.25 |
Frankreich will letztes Kohlekraftwerk auf Gas umstellen (dpa-AFX) | |
22.01.25 |
Schrott aus Atomanlagen am Rhein? Deutsche Seite skeptisch (dpa-AFX) | |
20.01.25 |
EDF-owned EV charge provider warns on weak UK retail demand (Financial Times) | |
14.01.25 |
French auditor recommends EDF delays UK Sizewell investment decision (Financial Times) | |
02.01.25 |
Frankreich exportiert Rekordmenge Strom auch an Deutschland (dpa-AFX) | |
18.12.24 |
Frankreich: Atommeiler startet mit zwölf Jahren Verspätung (dpa-AFX) | |
04.12.24 |
EDF to keep 4 UK nuclear power stations open longer than planned (Financial Times) | |
26.10.24 |
Atomkraft: Merz will mit Frankreich über Beteiligungen reden (dpa-AFX) |